Description

Heavy duties, High strength non-shrink Flow able Cementitious Grout.STONE GROUT GP-80 is a single component pre-weighed factory blended Non-shrink, high early strength free flow grout.

.


Pot Life @ 27 ºC temp: 15 minutes Compressive Strength: Age/ Days Compressive Strength in N/mm² W/P ratio: 0.18 (Flow able), (water curing after one day) 1 Day Approx.23 3Days Approx.53 7 days Approx.71.2 28 Days Approx.86.1 Note: Size of the cubes used 70.6mm x 70.6mm x 70.6mm tested at 30 ºC. Age/ Days Flexural Strength in N/mm² 7 Days > 9.2 28 Days > 11.1 Tensile Strength: > 3.87 N/mm² @7 days 5.60 N/mm² @ 28 days Unrestraint Expansion: 1.3% in plastic state. Flow characteristics: The maximum distance of flow is governed by the gap thickness, the head of the grout applied and the ambient temperature Yield: 13Lts at flow able consistency for 25 Kgs of HDPE bags Flexural Strength at 30 ºC: W/P ratio: 0.15 (Flowable), (Water curing after one day)

 Excellent flow characteristics
 Low creep characteristics under sustained loading.
 High Compressive, Tensile and Flexural strengths
  Non-shrink- and hence ensures complete surface contact
 and bond
 Suitable for a wide range of loading situations
 Does not shrink or over expand
 Chloride and iron free

 Precision grouting
 Grouting of base plates of turbines, compressors,boiler feed pumps
 Anchoring for a wide range of fixings.
 Masts, anchor bolts and fence posts.

25 Kgs HDPE bags.